Mix Chrome Plating Solution to 33Oz or 1000cc
![]() Click to enlarge |
|
Mix Chrome Plating Solution to 33Oz or 1000cc
Mix Chrome Plating Solution to 33 Oz
Combination chrome plated set mix Chrome plating into Water 1 liter. You will get the chrome plating solution volume to 1 liter or 33 Oz. Using the Anode is lead. Plating solution temperature 40-60 degrees. 4-15 DCv at 5-15 A/dm. Duration of 3-4 seconds, The importance plated chrome. To reduce the flow immediately before lifting work
How to use??. It before every treatment. Clean the most important piece of work prior to chrome plating. Before Plating Chrome. Specimens should be plated on the copper and nickel.!!
Equipment used in chrome express unit of electricity.
1. Power converter the current (Rectifier) for converting the AC power (AC) to be as the power flow. Direct (DC).
2. Tank plating using a coated steel cylinder internal unit lead (lead-lined steel) which is resistant to corrosion The first of Mick acid or chromate may tank made from a material Other resistant to corrosion.The complexity of the acid chromate Mick. Such as synthetic resin. (Synthetic resin sheets).
3. The positive electric pole (Anode) widely used lead This is great feature. is not soluble in acid and chromate deer. very high price not. While the pure lead can not be used The. Due to expensive and dissolved in acid. Chromate Mick the other unit. Or may lead mixed Antimony. Or lead-tin mixture. Which will decay before help organizations than the and are.
More robust than.
payment : Paypal
Shipping : Shipping by Airmail 11-20 Days
Write Review
Your Name:
Your Review: Note: HTML is not translated!
Rating: Bad Good
Enter the code in the box below:

Your Review: Note: HTML is not translated!
Rating: Bad Good
Enter the code in the box below:
There are no additional images for this product.

Categories
Information 

Shopping Cart