- PART A+ PART B + CM + your WATER(10000cc) = Liquid Chrome 10000cc (ready for use)
- Use with Lead or Tin anode
- Plated over Iron, Steel, Copper, Nickle, Silver, Gold, Aluminium ..etc
- Temperature normal or 38 - 60c. DC 4 - 15 v. After plating complete.
- Your parts dip into 3 - 4 second.